Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

The instrumental determination of hiding power quantifies a coating's ability to obliterate the color and contrast of the substrate beneath it, using reflectometry instead of subjective visual judgment. This article explains the contrast ratio method and the Kubelka-Munk approach described in ISO 6504 and ASTM D2805, covering sample preparation, instrumentation, calculation, and typical applications in coating quality control.

Technical Overview

Hiding power, also referred to as opacity or covering power, is the ability of a dry paint film to obscure the color or color differences of the substrate on which it is applied. It is one of the most important functional properties of architectural, industrial, and decorative coatings, because it directly determines how much paint must be applied to achieve a uniform appearance.

Instrumental determination replaces traditional visual comparison with objective photometric measurement. A film of the coating is applied at a defined thickness onto a substrate with contrasting black and white areas, and the reflectance of the dried film over each area is measured with a reflectometer or spectrophotometer. The ratio of reflectance over black to reflectance over white, known as the contrast ratio, provides a quantitative index of opacity. The principal standards governing this practice include ISO 6504-1 (Kubelka-Munk method for white and light-colored paints), ISO 6504-3 (contrast ratio at a fixed spreading rate), ASTM D2805 (hiding power by reflectometry), and GB/T 13452.3, the Chinese national method technically aligned with ISO 6504-1.

Testing Samples

Waterborne Architectural Coatings

Interior and exterior emulsion paints are the most frequently tested category. These products are typically evaluated at a fixed spreading rate such as 20 m²/L, and their hiding power is a key conformance parameter in national product standards for emulsion wall paints.

Solvent-Borne Decorative and Industrial Coatings

Alkyd enamels, primers, undercoats, and industrial topcoats can be assessed by the same reflectometric principle. For industrial systems, hiding power is often correlated with primer color and recommended dry film thickness in multi-coat specifications.

Sample Conditioning and Substrates

Prior to testing, samples shall be homogenized by stirring, freed from entrained air, and conditioned at 23 ± 2 °C and 50 ± 5 % relative humidity. Suitable substrates include commercially available black-and-white contrast charts of the type specified in the test standards, or clear glass panels measured in turn over black and white backing plates.

Testing Items

Depending on the selected method and product specification, the instrumental hiding power determination may include the following measurands:

  • Contrast ratio (CR) at a specified spreading rate, expressed as a percentage
  • Reflectance values of the dried film over black and over white substrates
  • Wet film thickness and dry film thickness verification
  • Spreading rate in m²/L at which 98 % contrast is achieved (full hiding)
  • Hiding power expressed as area per unit mass (m²/kg) for coatings specified on a mass basis
  • Derived Kubelka-Munk scattering and absorption coefficients for formulation studies

Testing Methods

Contrast Ratio Method (Reflectometry)

The coating is drawn down onto a black-and-white contrast chart using a film applicator or bar that produces the wet film thickness corresponding to the specified spreading rate. After drying under standard conditions and confirming complete film formation, the reflectance of the film over the black area and over the white area is measured with a reflectometer using standard illuminant D65 and the 10° standard observer, typically with d/8 geometry. The contrast ratio is calculated as CR = Y(black) / Y(white) × 100 %. A contrast ratio of 98 % or greater is conventionally regarded as full hiding.

Kubelka-Munk Method

For a more fundamental characterization, films are applied at several different thicknesses and their reflectances over black and over white are measured. Using the two-constant Kubelka-Munk theory, the scattering coefficient S and absorption coefficient K of the film are derived. From these values, the spreading rate required to reach a defined contrast ratio, usually 98 %, is calculated, giving hiding power in m²/L. This approach, specified in ISO 6504-1 and GB/T 13452.3, is applicable to white and light-colored paints and is particularly valuable for comparing pigment efficiency.

Instrumentation and Calibration

The measurement chain consists of a calibrated reflectometer or benchtop spectrophotometer, certified white working standards and a black cavity for zero verification, precision film applicators, and dry film thickness gauges. Instruments must be verified before each session, and the black and white areas of contrast charts should be checked for compliance with the reflectance tolerances stated in the method.

Expression of Results and Precision

Results are reported as the mean of at least duplicate determinations, together with the spreading rate or film thickness at which they were obtained. Repeatability depends strongly on the uniformity of the drawdown, the cleanliness of the substrate, and complete drying before measurement; these parameters must be controlled to obtain reproducible contrast ratio values.

Applications

Instrumental hiding power data support a wide range of practical activities in the coatings industry:

  • Production quality control and batch release for architectural and industrial paints
  • Formulation optimization, including titanium dioxide loading, extender selection, and pigment volume concentration tuning
  • Comparative evaluation of opacity pigments and opaque polymer additives
  • Incoming inspection of coating materials by contractors and accredited third-party laboratories
  • Conformance demonstration against product specifications such as national standards for interior and exterior emulsion coatings
  • Research and development studies correlating film morphology, thickness, and optical performance

FAQ

What does a contrast ratio of 98 % mean? It means the dried film reflects 98 % as much light over a black substrate as it does over a white substrate at the same spreading rate. At this level the substrate contrast is considered visually obliterated, which is the conventional criterion for full hiding.

Why use instrumental measurement instead of visual assessment? Visual hiding power evaluation is subjective and operator-dependent. Reflectometry provides traceable, reproducible numbers suitable for specification writing, arbitration, and statistical process control.

Which spreading rate is typically used? For architectural emulsion paints, 20 m²/L is the customary reference spreading rate, corresponding to a wet film thickness of approximately 50 µm, although other rates may be specified for particular product classes.

Is the method applicable to dark or strongly colored coatings? The Kubelka-Munk procedure of ISO 6504-1 is formally limited to white and light-colored paints because of the assumptions in the underlying optical theory. Dark and saturated colors can still be evaluated by direct contrast ratio measurement over black and white substrates, with measurement geometry and calibration chosen to suit the sample.

How should results be reported? The report should state the test standard applied, the spreading rate or film thickness, the measured reflectance values, the calculated contrast ratio or spreading rate at 98 % hiding, and the drying and conditioning conditions, so that results are comparable between laboratories.