Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Non-volatile content, often referred to as solids content, is one of the most fundamental quality parameters for coatings, resins, adhesives, inks and many chemical formulations, directly influencing formulation cost, film build and regulatory VOC declarations. This article provides a systematic evaluation of non-volatile content testing methods, comparing gravimetric oven techniques, vacuum drying and rapid instrumental approaches against international standards such as ISO 3251, ASTM D2369 and GB/T 1725. It also reviews sampling considerations, method validation criteria, typical applications and frequently asked questions to support laboratories and manufacturers in selecting the most appropriate test procedure.

Technical Overview

Non-volatile content (NV content) is defined as the mass percentage of a material that remains after a specimen is heated under specified conditions of temperature and time. It is an operationally defined parameter: the result depends not only on the sample itself but also on the drying conditions applied, because some low-boiling components may be retained while some thermally labile components may decompose, crosslink or polymerize during the test. For this reason, a meaningful evaluation of non-volatile content testing methods must consider both the measurement principle and the exact test conditions.

The dominant measurement principle is gravimetric: a weighed specimen is distributed in a tared dish, dried in a ventilated oven, cooled in a desiccator and reweighed. The non-volatile matter content is calculated as the ratio of the residue mass to the original specimen mass, expressed as a percentage by mass. Volatile content is then obtained by difference. The result is a key input for calculating VOC content according to ISO 11890-1, ISO 11890-2 and corresponding GB standards, and it is routinely used for quality control, batch release and supplier qualification in coatings and related industries.

Accredited third-party laboratories typically report non-volatile content with duplicate determinations and quoted repeatability limits, and they select the drying conditions according to the product standard or an agreed specification. Correct method selection and method evaluation are essential when results are used for regulatory declarations or commercial settlement.

Testing Samples

Coatings, Paints and Varnishes

Solvent-borne, water-borne, high-solids and radiation-curable liquid coatings are the largest application group. These products contain binders, pigments, fillers, additives and volatile solvents or water, and their non-volatile content typically ranges from about 30% to over 90% by mass. Powder coatings are also evaluated, usually after dispersion of the specimen in a volatile carrier to ensure uniform drying.

Resins, Binders and Polymer Dispersions

Liquid resins, resin solutions and aqueous polymer dispersions (latexes and emulsions) are tested to verify delivered solids and to control formulation stoichiometry. For dispersions, the formation of a continuous skin during drying can trap water, so thin, uniform specimen distribution and validated drying conditions are critical to avoid systematic under-reporting of volatility.

Adhesives and Sealants

Aqueous and solvent-borne adhesives, hot-melt prepolymers and reactive sealant systems are tested to determine applied solids and to predict shrinkage on cure. Two-component systems such as polyurethane or epoxy adhesives require testing immediately after mixing, since the reaction itself consumes volatile-free components and can distort results if delayed.

Printing Inks

Publication, packaging and screen-printing inks are evaluated for non-volatile content to control transfer solids, drying behavior and emission characteristics. High pigment loading means the specimen must be spread thinly and evenly to allow complete solvent removal.

Battery, Electronic and Specialty Materials

Electrode slurries, binder solutions, electronic encapsulants, electrolyte solvents and cleaning formulations are increasingly tested for non-volatile residue. For high-purity solvents, very low residue levels in the parts-per-million range are specified, requiring larger specimen masses and balances with appropriate resolution.

Testing Items

The core deliverables of a non-volatile content determination typically include:

  • Non-volatile matter content, expressed as percentage by mass of the specimen.
  • Volatile matter content, obtained by difference to 100%.
  • Volume solids, derived by combining non-volatile content with density measurements performed according to ISO 2811 or equivalent methods.
  • VOC content calculations for regulatory purposes, using non-volatile content as an input in combination with water content and density per ISO 11890-1, ISO 11890-2 or corresponding GB methods.
  • Precision indicators, including duplicate deviation and, where required, statements of repeatability and reproducibility.

Testing Methods

Oven Gravimetric Method (ISO 3251, ASTM D2369, GB/T 1725)

The reference method uses a forced-ventilation oven, an analytical balance with 0.1 mg readability and flat-bottom dishes made of aluminum, glass or stainless steel. A specimen, typically between 0.2 g and 1.5 g depending on the standard and expected solids level, is weighed into the tared dish and distributed as a thin, uniform layer. Optional dilution with a small amount of volatile solvent may be used for viscous or highly pigmented materials to improve film formation.

The dish is then heated at a specified temperature for a specified time, common combinations being approximately 105 °C for 60 minutes for many architectural coatings, 110 °C for 60 minutes for coatings per ASTM D2369, and temperatures between 125 °C and 160 °C for certain resins and industrial products where product standards or customer specifications dictate. After heating, the dish is cooled in a desiccator and reweighed. Duplicate determinations are performed, and results should agree within the repeatability limit stated in the method, typically on the order of 0.5 percentage points absolute or 2% relative for paint-like materials.

Vacuum Oven Method

For heat-sensitive materials such as certain acrylic dispersions, natural resins, pharmaceutical excipients and reactive prepolymers, drying under reduced pressure allows volatile removal at temperatures 30 to 60 degrees lower than atmospheric drying. The reduced boiling point of solvents and water under vacuum minimizes the risk of thermal degradation while still achieving complete removal of volatiles, although drying times may be extended.

Rapid Instrumental Methods

Halogen and infrared moisture analyzers with integrated balances provide results in five to twenty minutes and are widely used for in-process quality control. Thermogravimetric analysis (TGA) uses milligram-scale specimens and programmable heating ramps, making it valuable for method development because the mass-loss curve separates water, solvents and decomposition events. Both rapid techniques must be correlated against the reference oven method for each product family, and the correlation should be re-established whenever the formulation changes significantly.

Method Evaluation and Validation Criteria

A structured evaluation of non-volatile content methods should address the following parameters:

  • Trueness and bias: retained solvent due to skinning causes underestimation of volatility, while thermal degradation or oxidative crosslinking inflates the residue; both must be checked against reference conditions.
  • Precision: repeatability and reproducibility assessed according to ISO 5725 statistics, including interlaboratory comparisons or proficiency testing where available.
  • Robustness: sensitivity to deviations in oven temperature, drying time, specimen mass, film thickness and oven loading.
  • Applicability: reactive systems such as two-component polyurethanes, moisture-curing products and UV-curable formulations require agreed conditions, since the measured value represents non-volatile matter under the defined conditions rather than an absolute property.
  • Comparability: because non-volatile content is operationally defined, results are only comparable when temperature, time and specimen preparation are identical; standard selection must therefore be fixed in purchase specifications and test reports.

Applications

Non-volatile content data generated by validated methods support a wide range of technical and commercial decisions:

  • Regulatory VOC compliance declarations for architectural, industrial and consumer coatings under ISO 11890 and national GB limit standards.
  • Manufacturing quality control, including batch-to-batch solids adjustment, solvent addition control and yield accounting.
  • Formulation development, where volume solids govern theoretical spreading rate, hiding power and recommended film thickness.
  • Adhesive and sealant engineering, linking applied wet film to dry bondline thickness and predicting shrinkage.
  • Battery manufacturing, where slurry solids control areal mass loading of electrode coatings and process stability.
  • Incoming inspection and supplier qualification, with testing performed either in-house or by accredited third-party laboratories for independent verification.
  • Technical dispute resolution and export documentation, where standardized methods such as ISO 3251 provide a common contractual basis.

FAQ

What is the difference between non-volatile content and solids content?

The two terms are largely interchangeable in practice. Non-volatile content is the standards-based gravimetric result, while solids content is the colloquial industrial term. Strictly speaking, non-volatile content is defined by the specific drying conditions of the test method, so identical products tested under different conditions may yield slightly different values.

Which standard should be selected for testing?

ISO 3251 and GB/T 1725 are widely used for paints, varnishes and polymer dispersions, while ASTM D2369 is the common reference for coatings in North American supply chains. The choice should follow the product specification, the purchasing contract or the applicable regulatory scheme, and must be stated explicitly in the test report.

Why do oven results sometimes differ from moisture analyzer results?

Rapid infrared or halogen balances heat the specimen more aggressively and may trigger partial decomposition, or conversely may not fully remove high-boiling solvents within the short program. Correlating the instrumental method against the oven reference for each product family, and locking the drying program, keeps the deviation within acceptable limits.

What are the main causes of poor repeatability?

Frequent causes include non-uniform specimen spreading, excessive specimen mass leading to thick films and solvent entrapment, inadequate oven temperature uniformity, insufficient cooling time in the desiccator, moisture pick-up during weighing and premature testing of reactive two-component mixtures. Controlling specimen mass, film thickness and timing restores precision.

Can the method be applied to reactive or curing systems?

Yes, but the result must be interpreted as non-volatile matter under the agreed test conditions. For two-component or moisture-curing products, the specimen should be tested immediately after mixing, and for UV-curable materials, standards specific to radiation-curable products may apply to avoid mistaking conversion for evaporation.

How is non-volatile content used to calculate VOC content?

VOC calculations per ISO 11890-1 and ISO 11890-2 combine non-volatile content, water content and density to express VOC in grams per liter. Because any bias in the non-volatile determination propagates directly into the VOC result, laboratories handling compliance testing apply the strictest method controls and participate in regular interlaboratory verification.